Brazing & Soldering

APPLICATION DATA

No. 521 - Aluminum A/C Assembly

"Braze Mate" Model 150
Machine Specifications

Sequence:
1. Operator loads four tubes and block into stainless steel fixture.
2. Operator depresses touch switches to actuate automatic brazing cycle.
3. Two slide-mounted applicator guns advance to apply 4 identical paste deposits to joint areas, then retract.
4. Gas/air burners advance into position, adjust to high flame output and bring filler metal to brazing temperature.
5. Heat cycle times out, burners retract into low flame condition.
6. Timed air and water cooling.
7. Operator removes brazed assembly
Stainless steel fixture holds assembly in alignment throughout brazing cycle.
Premeasured deposits of aluminum paste filler metal are applied simultaneously to four joint areas.

FUSION INCORPORATED
4658 E. 355th St., Willoughby, OH 44094
Phone 1-800-626-9501 o (440) 946-3300
Fax (440) 942-9083 o e-mail: sales@fusion-inc.com